Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 20.9 MPa | 3030 psi | Optimum; With provided formulation; ASTM D638 |
PolyOne Geon™ 120 Series 121A Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 121A is high molecular weight resin providing good fused film physical properties. It provides good chemical foamability for producing medium to high density foams. It gives good dispersabili.. |