Polymer Property : Tensile Strength = 20.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 20.9 MPa
3030 psi
Optimum; With provided formulation; ASTM D638
PolyOne Geon™ 120 Series 121A Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® 121A is high molecular weight resin providing good fused film physical properties. It provides good chemical foamability for producing medium to high density foams. It gives good dispersabili..