Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 6.89 - 20.7 MPa | 1000 - 3000 psi | ASTM D638, ASTM D1709 |
Garlock 9405 PTFE Rubber Sheet, 25% Glass Filled Premium Grade 25% Glass-filled Skived PTFE SheetInformation provided by Garlock Rubber Technologies |