Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 30.00 MPa | 4351 psi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials Pearlthane® D91T86 Thermoplastic Polyurethane Type : Pearlthane® D91T86 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties... |