Lubrizol Advanced Materials Pearlthane® D91T86 Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlthane® D91T86 Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type : Pearlthane® D91T86 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties.Information provided by Merquinsa
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ISO 868
Tensile Strength 30.00 MPa
4351 psi
ISO 527-2/5A/500
Elongation at Break 800 %
800 %
ISO 527-2/5A/500
50% Modulus 0.00600 GPa
0.870 ksi
ISO 527-2/5A/500
100% Modulus 0.00600 GPa
0.870 ksi
ISO 527-2/5A/500
300% Modulus 0.0110 GPa
1.60 ksi
ISO 527-2/5A/500
Tear Strength 110 kN/m
628 pli
ISO 34-1B
Abrasion 22
22
[mm<sup>3</sup>]; ISO 4649-A
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C
185 °F
ISO 306
Processing Properties Metric English Comments
Feed Temperature 40.0 °C
104 °F
Nozzle Temperature 215 °C
419 °F
Zone 1 185 °C
365 °F
Zone 2 205 °C
401 °F
Zone 3 210 °C
410 °F
Zone 4 210 °C
410 °F
Dry Time 2.00 hour

@Temperature 80.0 °C
2.00 hour

@Temperature 176 °F
Descriptive Properties Value Comments
Compression Zone 205°C
Metering Zone 210°C