Polymer Property : Tensile Strength = 228 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 228 MPa
33100 psi
ASTM D-638
PlastiComp Complet® LGF50 - PA6 Nylon 6, 50% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementInformation provided by PlastiComp, Inc..
Tensile Strength 228 MPa
33100 psi
ASTM D-638
PlastiComp Complet® LGF60 - PA6 Nylon 6, 60% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 60% long glass reinforcementInformation provided by PlastiComp, Inc.
Tensile Strength 228 MPa
33100 psi
Conditioned; ASTM D638
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep ..
Tensile Strength 228 MPa
33000 psi
ASTM D638
Techmer ES HiFill FR® PC IM FR
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Tensile Strength 228 MPa
33000 psi
ASTM D638
Techmer ES Luriblend® PC IM FR
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Tensile Strength 228 MPa
33100 psi
ASTM D638
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned)
Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr..