Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 21.9 MPa | 3180 psi | ISO 527 |
S&E Specialty Polymers TufFillâ„¢ 5701 Black PP Application: High Calcium carbonate filed, high heat resistance thermoplastic extrusion grade based on polypropylene copolymer/homopolymer.Information provided by S&E Specialty Polymers |