Polymer Property : Tensile Strength = 20900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 144 MPa
20900 psi
at Break (NYP); ISO 527-1/-2
Quadrant EPP Ketron® CA30 PEEK + carbon fibres, extruded (ISO Data)
This 30 % carbon fibre reinforced grade combines even higher stiffness, mechanical strength and creep resistance than Ketron PEEK-GF30 with an optimum wear resistance. Moreover, compared with unrein..
Tensile Strength 144 MPa

@Temperature 150 °C
20900 psi

@Temperature 302 °F
ASTM D638
DuPont Performance Polymers VESPEL TP-8130 Polyimide
DuPont Vespel TP-8130 parts are specified for mechanical, thermal, and tribological properties. TP-8130 parts exhibits excellent strength and toughness, dimensional stability, low outgassing, radiat..