Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 144 MPa | 20900 psi | at Break (NYP); ISO 527-1/-2 |
Quadrant EPP Ketron® CA30 PEEK + carbon fibres, extruded (ISO Data) This 30 % carbon fibre reinforced grade combines even higher stiffness, mechanical strength and creep resistance than Ketron PEEK-GF30 with an optimum wear resistance. Moreover, compared with unrein.. |
|||
Tensile Strength | 144 MPa @Temperature 150 °C |
20900 psi @Temperature 302 °F |
ASTM D638 |
DuPont Performance Polymers VESPEL TP-8130 Polyimide DuPont Vespel TP-8130 parts are specified for mechanical, thermal, and tribological properties. TP-8130 parts exhibits excellent strength and toughness, dimensional stability, low outgassing, radiat.. |