Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 206 MPa | 29900 psi | ASTM D638 |
Quantum Composites LYTEX® 4181 55% Carbon Fiber Reinforced Epoxy SMC LYTEX 4181 is an epoxy ESC molding compound designed for structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance.. |
|||
Tensile Strength | 206 MPa | 29900 psi | 50 mm/min; ISO 527-1,-2 |
Gromax BFG45-AS00N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Strength | 206 MPa | 29900 psi | 50 mm/min; ISO 527-1,-2 |
Gromax BFG45-B100N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |