Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 2.40 MPa @Strain 100 % |
348 psi @Strain 100 % |
ISO 37 |
BASF Elastollan S 60 A SPF TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 2.40 MPa | 348 psi | average; in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® R63.140 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable.. |
|||
Tensile Strength | 2.40 MPa | 348 psi | Measured on compression molded slabs; ISO 37 |
Kraton® D1119 B (SIS) Linear Triblock Copolymer Description: Kraton D1119 B is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from South America in the physical form identified: .. |
|||
Tensile Strength | 2.40 MPa | 348 psi | Typical properties on film cast from toluene solution; ASTM D412 |
Kraton® D1119 P (SIS) Linear Triblock Copolymer Description: Kraton D1119 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified: .. |
|||
Tensile Strength | 2.40 MPa | 348 psi | ISO 37 |
AlphaGary Evoprene™ GC 5694 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |