Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1330 MPa @Treatment Temp. 500 °C |
193000 psi @Treatment Temp. 932 °F |
42 HRC |
Schmolz + Bickenbach Cryodur® 2312 (Brake Die) Cold Work Die Steel Description: Cryodur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared t.. |
|||
Tensile Strength | 1330 MPa @Treatment Temp. 500 °C |
193000 psi @Treatment Temp. 932 °F |
42 HRC |
Schmolz + Bickenbach Formadur® 2311 Plastic Mold Steel Description: Formadur® 2311 is a pre-hardened plastic mold steelCharacteristics: Good texturing compared to Formadur®2312 and Good polishability compared to Formadur® 231Applications: Injection m.. |
|||
Tensile Strength | 1330 MPa @Treatment Temp. 500 °C |
193000 psi @Treatment Temp. 932 °F |
42 HRC |
Schmolz + Bickenbach Formadur® 2312 (Ultra Holder) Plastic Mold Steel Description: Formadur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared .. |