Mechanical Properties Metric English Comments
Tensile Strength 186 MPa
27000 psi
ASTM D-638
PlastiComp Complet® LCF40-PEI Polyetherimide, 40% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyetherimide with 40% long carbon fiber reinforcementInformation provided by PlastiC..
Tensile Strength 186 MPa
27000 psi
ASTM D638
Kolon KOPA® KN333G30BL G/F Reinforced Nylon 66
G/F 30% reinforcedApplications Engine coversInformation provided by API-Kolon.
Tensile Strength 186 MPa
27000 psi
ASTM D638
Kolon KOPA® KN333G30CRN G/F Reinforced Nylon 66
Oil resistantApplications Surge tanksInformation provided by API-Kolon.
Tensile Strength 186 MPa
27000 psi
ASTM D638
Kolon KOPA® KN333G35CR G/F Reinforced Nylon 66
High thermal resistant, Weather resistant, dimensionally stableApplications Cylinder head coversInformation provided by API-Kolon.
Tensile Strength 186 MPa
27000 psi
ASTM D638
Kolon KOPA® KN333G35CRBK G/F Reinforced Nylon 66
EG-resistant, high strength, dimensionally stableApplications Coolant temperature control partsInformation provided by API-Kolon.
Tensile Strength 186 MPa
27000 psi
ASTM D638
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® BR42B 40% glass fiber reinforced polyphenylene sulfide compound is specially formulated to provide low coefficient of friction and reduced wear rate for use in applications requiring low s..
Tensile Strength 186 MPa
27000 psi
ASTM D638
Solvay Specialty Polymers Ryton® R-4-222NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-222NA 40% glass fiber reinforced polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water and complies with Un..
Tensile Strength 186 MPa
27000 psi
ASTM D638
Shinkong Synthetic Fibers Shinite® N601G30 Nylon 66, 30% Glass Filled
Information from Shinkong Synthetic Fibers Corp.
Tensile Strength 186 MPa
27000 psi
ASTM D638
Shinkong Synthetic Fibers Shinite® N601G30 Nylon 66, 30% Glass Filled
Information from Shinkong Synthetic Fibers Corp.
Tensile Strength 186 MPa
27000 psi
ASTM D638
Solvay Specialty Polymers Ryton® R-4-220NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur..
Tensile Strength 186 MPa
27000 psi
GB/T 1040.2-2006
Sichuan Deyang Haton® hMR61LC1 Polyphenylene Sulfide, Glass & Mineral Reinforced
Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD