Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 127.53 MPa | 18497 psi | ASTM D638 |
E-Polymers SEPAZ® LC50 PP Copolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Tensile Strength | 127.53 MPa | 18497 psi | ASTM D638 |
E-Polymers TEKAMID® HG20L 20% Glass Fiber Reinforced High Impact PA/ABS Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB.. |
|||
Tensile Strength | 127.53 MPa | 18497 psi | ASTM D638 |
E-Polymers SEPAZ® C130M 30% Mineral Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |