Polymer Property : Tensile Strength = 18.032 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 18.032 MPa

@Temperature 136 °C,
Time 605000 sec
2615.3 psi

@Temperature 277 °F,
Time 168 hour
Aged, 30 mil dumbbell speciment
S&E Specialty Polymers TufTech™ GA-1050-02LF PVC Compound
Application: A 105°C, AWM, 90°C AWM 1,000 volt, flame retardant compound.Information provided by S&E Specialty Polymers