Material Notes:
Application: A 105°C, AWM, 90°C AWM 1,000 volt, flame retardant compound.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.36 g/cc
1.30 - 1.36 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 90.0 - 96.0
90.0 - 96.0
ASTM D2240
Tensile Strength 18.4 MPa
2670 psi
ASTM D412
18.032 MPa

@Temperature 136 °C,
Time 605000 sec
2615.3 psi

@Temperature 277 °F,
Time 168 hour
Aged, 30 mil dumbbell speciment
Elongation at Break 300 %
300 %
ASTM D412
255 %

@Treatment Temp. 136 °C,
Time 605000 sec
255 %

@Treatment Temp. 277 °F,
Time 168 hour
Aged, 30 mil dumbbell speciment
Thermal Properties Metric English Comments
Oxygen Index >= 28.0 %
>= 28.0 %
ASTM D2863