Mechanical Properties Metric English Comments
Tensile Strength 11.57 MPa
1678 psi
ASTM D412
Elastocon TPE Technologies Elastocon® OF75 Thermoplastic Elastomer
Elastocon® OF75 is a natural thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, high strength properties and a reduced coefficient of friction. Ela..