Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 11.57 MPa | 1678 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® OF75 Thermoplastic Elastomer Elastocon® OF75 is a natural thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, high strength properties and a reduced coefficient of friction. Ela.. |