Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1570 MPa @Treatment Temp. 300 °C |
228000 psi @Treatment Temp. 572 °F |
48 HRC |
Schmolz + Bickenbach Cryodur® 2312 (Brake Die) Cold Work Die Steel Description: Cryodur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared t.. |
|||
Tensile Strength | 1570 MPa @Treatment Temp. 300 °C |
228000 psi @Treatment Temp. 572 °F |
48 HRC |
Schmolz + Bickenbach Formadur® 2311 Plastic Mold Steel Description: Formadur® 2311 is a pre-hardened plastic mold steelCharacteristics: Good texturing compared to Formadur®2312 and Good polishability compared to Formadur® 231Applications: Injection m.. |
|||
Tensile Strength | 1570 MPa @Treatment Temp. 300 °C |
228000 psi @Treatment Temp. 572 °F |
48 HRC |
Schmolz + Bickenbach Formadur® 2312 (Ultra Holder) Plastic Mold Steel Description: Formadur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared .. |
|||
Tensile Strength | 1570 MPa | 227000 psi | 48 HRC |
Schmolz + Bickenbach Thermodur® 2343 EFS Extra Fine Structure (H-11)- Hot Work Die Steel Description: Thermodur® 2343 is a single melt Extra Fine Structure (EFS) hot work die steel and Supplied in the annealed conditionCharacteristics: Good toughness; Moderate high-temperature strength.. |