Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 155 MPa | 22500 psi | ASTM D638 |
PlastiComp Complet® LGF30-PA66 MT 30% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |