Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 80.0 - 100 MPa | 11600 - 14500 psi | Compression; ISO 527 |
Raschig Group RESINOL® 87120 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Tensile Strength | 70.0 - 100 MPa | 10200 - 14500 psi | Compression; ISO 527 |
Raschig Group RALUPOL® 8605 UP Polyester Glass fiber reinforced polyester molding compound. Resistant to hydrolysis. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU dire.. |