Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 8.998 MPa | >= 1305 psi | ASTM F152 |
Thermoseal RG-N120 PTG Gasketing Thermoseal RG-N120 is a reinforced cellulose gasket material with a nitrile butadiene rubber binder and inorganic fillers that provides a very good crush resistance at high flange pressures. Continu.. |