Material Notes:
Thermoseal RG-N120 is a reinforced cellulose gasket material with a nitrile butadiene rubber binder and inorganic fillers that provides a very good crush resistance at high flange pressures. Continuous roll lengths allow efficient and economical fabrication with high speed die cutting equipment. RG-N120 seals oil, water, and coolants w ell in applications such as small engine intake and cover gaskets, automotive water pump and throttle body gaskets and similar applications with intermittent operating temperatures up to 350° F (177° C).Information provided by Thermoseal Inc.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM F1315
Thickness 800 microns
31.5 mil
Thickness tested
Mechanical Properties Metric English Comments
Tensile Strength >= 8.998 MPa
>= 1305 psi
ASTM F152
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
350 °F
intermittent
Descriptive Properties Value Comments
Binder Type Nitrile Butadiene Rubber
Compressibility 25-35 percent
ASTM F36J
Recovery >30 percent
ASTM F36J
Thickness Increase <10%
After immersion in Fuel B
<15%
After immersion in Oil IRM903
Weight Increase <10%
After immersion in Oil IRM903
<30%
After immersion in Fuel B