Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 850 MPa | 123000 psi | |
H.C. Starck HPM 1700 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Tensile Strength | 850 MPa | 123000 psi | |
H.C. Starck HPM 1710 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Tensile Strength | 848 MPa @Treatment Temp. 700.0 °C |
123000 psi @Treatment Temp. 1292 °F |
28 HRC |
Schmolz + Bickenbach Cryodur® 2312 (Brake Die) Cold Work Die Steel Description: Cryodur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared t.. |
|||
Tensile Strength | 848 MPa @Treatment Temp. 700.0 °C |
123000 psi @Treatment Temp. 1292 °F |
28 HRC |
Schmolz + Bickenbach Formadur® 2311 Plastic Mold Steel Description: Formadur® 2311 is a pre-hardened plastic mold steelCharacteristics: Good texturing compared to Formadur®2312 and Good polishability compared to Formadur® 231Applications: Injection m.. |
|||
Tensile Strength | 848 MPa @Treatment Temp. 700.0 °C |
123000 psi @Treatment Temp. 1292 °F |
28 HRC |
Schmolz + Bickenbach Formadur® 2312 (Ultra Holder) Plastic Mold Steel Description: Formadur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared .. |