Polymer Property : Tensile Strength = 113 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 113 MPa
16400 psi
ASTM D638
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a low ..
Tensile Strength 113 MPa
16400 psi
ASTM D638
Gromax PET 9030-104E 30% Glass/Mineral Filled
Product Description: PET glass 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellent wear..
Tensile Strength 113 MPa
16400 psi
50 mm/min; ISO 527
Gromax BTG30-DN03N1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Tensile Strength 113 MPa
16400 psi
ASTM D638
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI)
Torlon® 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a ..
Tensile Strength 113 MPa
16400 psi
ASTM D638
Shinkong Synthetic Fibers Shinite® F102G30 PET, 30% Glass Filled, Fire Retardant, Halogen Free
Information from Shinkong Synthetic Fibers Corp.
Tensile Strength 113 MPa
16400 psi
ASTM D638
Shinkong Synthetic Fibers Shinite® F102G30 PET, 30% Glass Filled, Fire Retardant, Halogen Free
Information from Shinkong Synthetic Fibers Corp.
Tensile Strength 113 MPa
16400 psi
DIN EN ISO 527
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced
Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex
Tensile Strength 113 MPa
16400 psi
ASTM D638
Gromax CCP PET 9130-200 30% Glass Filled
Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell..