Polymer Property : Tensile Strength = 1070 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 7.40 MPa
1070 psi
Flatwise
Henkel Hysol PL 780-1 Film Adhesive
Nonmetallic, toughened, modified epoxy film designed for bonding metal, composite and thermoplastic structures. High shear properties at 350°F / 177°C. Excellent hot-wet properties. High flow ..
Tensile Strength 7.40 MPa
1070 psi
Flatwise
Henkel Hysol PL 7000 Film Adhesive
Epoxy film adhesive formulated to provide excellent performance properties in composite bonding, and has excellent results on composite surfaces that have been exposed to bond shop environments and ..
Tensile Strength 7.40 MPa
1070 psi
perpendicular to plane; ASTM C297
3A Composites Core Materials BALTEK® SB.50 Structural End-Grain Balsa
BALTEK SB is a core material produced from certified kiln-dried balsa wood in the ‘end-grain’ confiation. It has extremely high strength and stiffness to weight ratios, and achieves an excellent b..
Tensile Strength 7.40 MPa
1070 psi
ISO 37
AlphaGary Evoprene™ Super G 948 SEBS Thermoplastic Elastomer
Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties..