Polymer Property : Tensile Strength = 105 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 105 MPa
15200 psi
at Yield; ISO 527-1/-2
Quadrant EPP Ertalon® 4.6 PA 4.6, extruded (ISO Data)
Compared with conventional nylons, Ertalon 4.6 features a better retention of stiffness and creep resistance over a wide range of temperatures as well as superior heat ageing resistance. Therefore, ..
Tensile Strength 105 MPa
15200 psi
ASTM D638
Quantum PEI - Ultem®
Information provided by Quantum Advanced Engineering Plastics
Tensile Strength 105 MPa
15200 psi
ASTM D638
Quantum Composites QC-8777 41% Glass Fiber Reinforced Polyester Hybrid SMC
QC-8777 is a polyester hybrid engineered structural composite molding compound designed for compression molding of components requiring high structural strength, corrosion resistance and temperature..
Tensile Strength 105 MPa
15200 psi
DIN 53455
Isoflon PEI Polyetherimide
Materials with strong mechanical and electrical performances under high temperatures.Information provided by Isoflon.
Tensile Strength 105 MPa
15300 psi
ASTM D638
Ensinger Tecapeek® XP-102 Compression Molded PEEK Compound, Filled with 15% Graphite and 10% PTFE
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Tensile Strength 105 MPa
15200 psi
ASTM D638
E-Polymers TEKAMID® TA210MS MoS2 Filled PA66 Resin
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,..
Tensile Strength 105 MPa

@Temperature 23.0 °C
15200 psi

@Temperature 73.4 °F
DAM; ASTM D638
DuPont Performance Polymers Minlon® FE6190 BK086 Nylon 66
Minlon® FE6190 BK086 is a 36% mineral/glass reinforced, heat stabilized, black polyamide resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength 105 MPa
15200 psi
dry; ISO 527
Azoty Tarnow™ Tarnamid® T-27 GF10 MX10 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grade, reinforced with 10% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good surface quality.T..
Tensile Strength 105 MPa
15200 psi
cond.; ISO 527
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Tensile Strength 105 MPa
15200 psi
cond.; ISO 527
Azoty Tarnow™ Tarnamid® T-27 GF30 I Polyamide 6 - Glass Fiber Reinforced
30% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai..
Tensile Strength 105 MPa
15200 psi
cond.; ISO 527
Azoty Tarnow™ Tarnamid® T-27 GF40 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 40% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Tensile Strength 105 MPa
15200 psi
ASTM D638
Gharda Chemicals G-PAEK™ 1200P Ultra High Performance PEK Polymer
Product Details: Ultra High performance thermoplastic material, unreinforced Poly Aryl Ether Ketone (G-PAEK), semi-crystalline, coarse powder for extrusion compounding, FDA food contact compliant, ..