Category Polymer , Thermoplastic , Polyketone
Manufacturer Gharda Chemicals
Trade Name G-PAEK™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gharda Chemicals G-PAEK™ 1200P Ultra High Performance PEK Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Details: Ultra High performance thermoplastic material, unreinforced Poly Aryl Ether Ketone (G-PAEK), semi-crystalline, coarse powder for extrusion compounding, FDA food contact compliant, easy flow, Color natural milky whiteParticle Size Distribution: D(0.1)
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
Viscosity 200 cP

@Shear Rate 1000 1/s
200 cP

@Shear Rate 1000 1/s
CR Viscosity at 6 Min; Capillary Rheometer
Crystallinity 40 %
40 %
DSC
Mechanical Properties Metric English Comments
Tensile Strength 105 MPa
15200 psi
ASTM D638
Elongation at Break 10 - 15 %
10 - 15 %
ASTM D638
Tensile Modulus 4.20 GPa
609 ksi
ASTM D638
Flexural Strength 185 - 190 MPa
26800 - 27600 psi
ASTM D790
Flexural Modulus 4.10 GPa
595 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 370 - 372 °C
698 - 702 °F
DSC
Glass Transition Temp, Tg 152 - 154 °C
306 - 309 °F
DSC/onset
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
Users viewing this material also viewed the following: