Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 103 MPa | 14900 psi | ASTM D638 |
PolyOne Stat-Tech™ LC-20NCF/000 V3 RD 4020 Liquid Crystal Polymer (LCP) Information provided by PolyOne |
|||
Tensile Strength | 103 MPa | 15000 psi | ASTM D638 |
Quadrant EPP Nylatron® 4.6 (ASTM Product Data Sheet) |
|||
Tensile Strength | 103 MPa | 15000 psi | ASTM D638 |
Quadrant EPP Semitron® MPR-1000 (ASTM Product Data Sheet) |
|||
Tensile Strength | 103 MPa | 15000 psi | ASTM D638 |
Quadrant EPP Duratron® PAI T5530 Compression Molded Glass Reinforced Polyamide-imide (ASTM Product Data Sheet) |
|||
Tensile Strength | 103 MPa | 14900 psi | ASTM D638 |
Solvay Specialty Polymers Mindel® B-322 Polysulfone, Modified (PSU, Modified)
(discontinued **) Mindel B-322 is a glass filled, modified polysulfone developed specifically for molded electrical connector applications requiring excellent dimensional stability and resistance to warpage. This mat.. |
|||
Tensile Strength | 103 MPa | 14900 psi | ASTM D638 |
Kolon SPESIN® KP213G15SIBL Glass Fiber Reinforced PBT Compound Resin G/F 15%, high toughness, excellent surfaceApplications: Various types of housingsInformation provided by API-Kolon. |
|||
Tensile Strength | 103 MPa | 14900 psi | ASTM D638 |
Solvay Specialty Polymers Ryton® XE5515BL Polyphenylene Sulfide Alloy (PPS Alloy), 15% Glass Fiber Ryton® XE5515BL 15% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength and chemical resistance at elevated temperatures and is suitable for extrusi.. |
|||
Tensile Strength | 103 MPa | 15000 psi | ASTM D638 |
Ensinger Tecapeek® XP-92 Compression Molded PEEK Compound, 15% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Strength | 103 MPa | 15000 psi | in plane |
Carlisle 201HD Carbon-Carbon Composite Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t.. |
|||
Tensile Strength | 103 MPa | 14900 psi | Machine; ASTM D882 |
Arlon DiClad 870 PTFE/Woven Fiberglass Laminate Extremely Low Loss TangentExcellent Dimensional StabilityProduct Performance UniformityBenefits:Electrical Properties are highly uniform across frequencyConsistent Mechanical PerformanceExcellent Ch.. |
|||
Tensile Strength | 103 MPa | 15000 psi | Cross; ASTM D882 |
Arlon DiClad 522/527 PTFE/Woven Fiberglass Laminates DiClad 522 and DiClad 527 use a higher fiberglass/PTFE ratio to provide mechanical properties approaching conventional substrates.Extremely Low Loss TangentExcellent Dimensional StabilityProduct Per.. |
|||
Tensile Strength | 103 MPa | 15000 psi | in plane |
Carlisle 201LD Carbon-Carbon Composite Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t.. |
|||
Tensile Strength | 103 MPa | 15000 psi | ASTM D638 |
Quadrant EPP Duratron® PAI T4301 Polyamide-imide, extruded bearing grade (ASTM Product Data Sheet) |
|||
Tensile Strength | 103 MPa | 14900 psi | |
Lucite International Elvacite ® 2021 Acrylic Resin Elvacite® 2021 is a high molecular weight methyl methacrylate polymer. It is used in barrier coatings for vinyl. Its high molecular weight provides excellent abrasion resistance.Information provide.. |