Polymer Property : Tensile Strength = 10.21 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 10.21 MPa
1481 psi
Silicone Property; Arlon SQA-TMS-008
Arlon 90B32R016AC Aluminum Clad Press Pad with "C-Finish"
Design/Construction:Side 2: Alloy 1100 Aluminum FoilSide 1: Cured Silicone RubberThis data represents typical values for the production material and should not be used as material specifications.I..
Tensile Strength 10.21 MPa
1481 psi
Silicone Property; Arlon SQA-TMS-008
Arlon 91B32R016AC Aluminum Clad Silicone Press Pad with "C-finish"
Design/Construction:Side 2: Alloy 1100 H18 Aluminum FoilSide 1: Cured Silicone RubberThis data represents typical values for the production material and should not be used as material specificatio..