Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1.43 MPa @Temperature 22.0 °C, Time 252000 sec |
207 psi @Temperature 71.6 °F, Time 70.0 hour |
50% RH, Exposure to Carpet Cleaner; ASTM D412 |
Parker Chomerics CHO-SEAL S6305 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded and Extruded.RoHS CompliantInformation provi.. |
|||
Tensile Strength | 1.43 MPa @Temperature 22.0 °C, Time 252000 sec |
207 psi @Temperature 71.6 °F, Time 70.0 hour |
50% RH, Exposure to Hairspray; ASTM D412 |
Parker Chomerics CHO-SEAL S6305 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded and Extruded.RoHS CompliantInformation provi.. |
|||
Tensile Strength | 1.43 MPa @Temperature 22.0 °C, Time 252000 sec |
207 psi @Temperature 71.6 °F, Time 70.0 hour |
50% RH, Exposure to Windshield Washer Solvent; ASTM D412 |
Parker Chomerics CHO-SEAL S6305 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded and Extruded.RoHS CompliantInformation provi.. |