Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 0.485 MPa | 70.3 psi | ISO 7214 1998 |
Zotefoams Evazote® VA25 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |