Mechanical Properties Metric English Comments
Tensile Strength 0.300 - 0.390 MPa
43.5 - 56.6 psi
DIN 53455
Isoflon PUR Polyurethane
Very high wear resistanceHighly resilientInformation provided by Isoflon.
Tensile Strength 0.300 MPa
43.5 psi
ISO 7214 1998
Zotefoams Plastazote® LD18 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Tensile Strength 0.300 MPa
43.5 psi
DIN EN ISO 1798
BASF Neopolen® P 8015 0.02 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8015 is expanded Polypropylene supplied in the form of beads. The cells are largely closed. Physical properties of moldings made from Neopolen® P 8015Note: In order to mea..
Tensile Strength 0.300 MPa
43.5 psi
DIN EN ISO 1798
BASF Neopolen® P 8220 K 0.02 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to..
Tensile Strength 0.300 MPa
43.5 psi
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..