Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength, Total | 350 N | 78.7 lb (f) | ASTM D1004 |
Eastman Eastman AP006 Copolyester Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly.. |
|||
Tear Strength, Total | 350 N | 78.7 lb (f) | ASTM D1004 |
Eastman Eastman AP007 Copolyester Applications:Automotive componentsBreathable filmsElectronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsOffice furniturePackagingPolymer modificationProfilesRubber an.. |
|||
Tear Strength, Total | 350 N | 78.7 lb (f) | ASTM D1004 |
Eastman Neostar FN006 Elastomer Neostar FN006 elastomer is the second in Eastman’s series of tough, clear, durable copolyester ethers. Developed for use in the profile and automotive markets, it can also be used in packaging and .. |
|||
Tear Strength, Total | 350 N | 78.7 lb (f) | ASTM D1004 |
Eastman Neostar FN007 Elastomer Neostar FN007 elastomer is the third in Eastman’s series of tough, clear, durable copolyester ethers. Though originally designed for use in the profile and automotive markets, this innovative copol.. |