Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Neostar FN006 Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester TPE , Polyester, TP
Manufacturer Eastman Chemical
Trade Name Neostar
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Neostar FN006 Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Neostar FN006 elastomer is the second in Eastman’s series of tough, clear, durable copolyester ethers. Developed for use in the profile and automotive markets, it can also be used in packaging and tubing applications. Its chemical resistance, flexibility, and toughness make it an ideal choice for applications where strength, durability, and puncture resistance in harsh environments is required. Neostar FN006 can be used in injection molding or cast film, blown film, or tubing extrusion applications. This copolyester has a full range of flexibility and memory without the addition of plasticizers. Considered environmentally preferred due to its non-halogenated material composition, it can be incinerated cleanly without the emission of toxic gases. The target inherent viscosity of this product is 1.6.Applications/UsesAutomotiveFlexible hingesPricing channelsRetail pricing finsDriver and passenger side air bagsPackagingProfilesTubingKey AttributesEnvironmentally preferred, non-halogenated materialExcellent chemical resistanceExceptional heat resistance and high temperature dimensional stabilityHigh flexibility without plasticizersSolvent bondable
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Water Absorption 0.40 %
0.40 %
24h Immersion; ASTM D570
Viscosity Measurement 1.16
1.16
Inherent; EMN-A-AC-G-V-1
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength at Break 22.0 MPa
3190 psi
ASTM D638
Tensile Strength, Yield 14.0 MPa
2030 psi
ASTM D638
Elongation at Break 400 %
400 %
ASTM D638
Elongation at Yield 38 %
38 %
ASTM D638
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D638
Flexural Modulus 0.150 GPa
21.8 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm

@Temperature -40.0 °C
0.749 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Tear Strength, Total 350 N
78.7 lb (f)
ASTM D1004
Thermal Properties Metric English Comments
Heat of Fusion 27.0 J/g
11.6 BTU/lb
ASTM E793
CTE, linear 150 µm/m-°C

@Temperature 20.0 °C
83.3 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.60 J/g-°C
0.382 BTU/lb-°F
DSC
1.80 J/g-°C

@Temperature 100 °C
0.430 BTU/lb-°F

@Temperature 212 °F
DSC
2.00 J/g-°C

@Temperature 150 °C
0.478 BTU/lb-°F

@Temperature 302 °F
DSC
2.30 J/g-°C

@Temperature 175 °C
0.550 BTU/lb-°F

@Temperature 347 °F
solid; DSC
2.30 J/g-°C

@Temperature 225 °C
0.550 BTU/lb-°F

@Temperature 437 °F
melt; DSC
3.10 J/g-°C

@Temperature 200 °C
0.741 BTU/lb-°F

@Temperature 392 °F
transition; DSC
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 205 °C
401 °F
Crystalline Peak Melting Point; ASTM D3418
Crystallization Temperature 140 °C
284 °F
on cooling; DSC
Vicat Softening Point 170 °C
338 °F
1kg load; ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Glass Transition Temp, Tg -3.00 °C
26.6 °F
DSC
Clash Berg Stiffness Temperature <= -70.0 °C
<= -94.0 °F
at 930 MPa; ASTM D1043
-28.0 °C
-18.4 °F
at 240 MPa; ASTM D1043
Copyright © lookpolymers.com All Rights Reserved