Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength, Total | 66.0 N | 14.8 lb (f) | T.D., PPT; ASTM D2582 |
Eastman Eastman Embrace Copolyester for Extrusion/Cast Film Applications:Flexible packagingIV containersLabels to fit high contour containersShrink packagingWrap around designKey Attributes:Excellent clarityExcellent printabilityGood chemical resistanceGood .. |