Mechanical Properties Metric English Comments
Tear Strength, Total 66.0 N
14.8 lb (f)
T.D., PPT; ASTM D2582
Eastman Eastman Embrace Copolyester for Extrusion/Cast Film
Applications:Flexible packagingIV containersLabels to fit high contour containersShrink packagingWrap around designKey Attributes:Excellent clarityExcellent printabilityGood chemical resistanceGood ..