Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength, Total 2.40 N
0.540 lb (f)
MD; ISO 6383/2
Borealis Himod™ FT3280 LDPE for Film
Himod FT3280 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Tear Strength, Total 2.40 N
0.540 lb (f)
M.D., Elmendorf; ASTM D1922
Eastman Embrace LV Copolyester for Shrink Film
Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo..