Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength, Total | 2.10 N | 0.472 lb (f) | TD; ISO 6383/2 |
Borealis Himodâ„¢ FT3280 LDPE for Film Himod FT3280 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |