Polymer Property : Tensile Impact = 74.7 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact 74.7 J/cm
140 ft-lb/in
ASTM D1822
LyondellBasell Alathon® L5840 High Density Polyethylene
ApplicationsALATHON L 5840 is a lightweight resin that exhibits excellent color, low odor and provides processing stability. Typical applications include household chemicals, industrial chemicals, ..