Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 74.7 J/cm | 140 ft-lb/in | ASTM D1822 |
LyondellBasell Alathon® L5840 High Density Polyethylene ApplicationsALATHON L 5840 is a lightweight resin that exhibits excellent color, low odor and provides processing stability. Typical applications include household chemicals, industrial chemicals, .. |