Polymer Property : Tensile Impact = 656 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact 350 J/cm
656 ft-lb/in
ASTM D4272
Iran Petrochemical (PCC) 2100TN00 Low Density Polyethylene
LDPE 2100TN00: Heavy duty film suitable for application in shrink hoods, industrial sacks, heavy duty carrier bags and liners.Information provided by Iran Petrochemical Commercial Co.