  Online Service   lookpolymers   27660005
Material Notes:
LDPE 2100TN00: Heavy duty film suitable for application in shrink hoods, industrial sacks, heavy duty carrier bags and liners.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ISO 1183
Melt Flow 0.30 g/10 min
0.30 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ISO R527-1
Film Tensile Strength at Yield, TD 11.0 MPa
1600 psi
ISO R527-1
Film Elongation at Break, MD >= 200 %
>= 200 %
ISO R527-1
Film Elongation at Break, TD >= 500 %
>= 500 %
ISO R527-1
Modulus of Elasticity 0.180 GPa
26.1 ksi
MD; ISO R527-1
0.190 GPa
27.6 ksi
TD; ISO R527-1
Tensile Impact 350 J/cm
656 ft-lb/in
ASTM D4272
Coefficient of Friction 0.70
0.70
ASTM D1894
Tear Strength 20.0 kN/m
114 pli
MD; ISO 6383-2
25.0 kN/m
143 pli
TD; ISO 6383-2
Film Tensile Strength at Break, MD 29.0 MPa
4210 psi
ISO R527-1
Film Tensile Strength at Break, TD 26.0 MPa
3770 psi
ISO R527-1
Optical Properties Metric English Comments
Haze 15 %
15 %
ASTM D1003A
Gloss 39 %
39 %
ASTM D2457
Descriptive Properties Value Comments
Clarity, mV 56
Sabtec