Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 300 J/cm | 562 ft-lb/in | ASTM D4272 |
Iran Petrochemical (PCC) 2101TN47 Low Density Polyethylene LDPE 2101TN47 Shrink FilmThis grade enables high speed production of film without blocking.Information provided by Iran Petrochemical Commercial Co. |
|||
Tensile Impact | 300 J/cm | 562 ft-lb/in | ASTM D4272 |
Iran Petrochemical (PCC) LH0030 Low Density Polyethylene LH0030 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Applications: general packaging applications, part.. |
|||
Tensile Impact | 300 J/cm | 562 ft-lb/in | ASTM D4272 |
Iran Petrochemical (PCC) LS0085/KJ Low Density Polyethylene LS0085/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Application: shrink packaging.Information prov.. |