Mechanical Properties Metric English Comments
Tensile Impact 374 J/cm
700 ft-lb/in
Warp
Hexcel® HexForce™ 328 Aramid Fabric
Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid..
Tensile Impact 374 J/cm
700 ft-lb/in
Warp Breaking Strength
Hexcel® HexForce™ 3582 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Tensile Impact 374 J/cm
700 ft-lb/in
Warp
Hexcel® HexForce™ 5328 Aramid Fabric
Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid..
Tensile Impact 374 J/cm
700 ft-lb/in
Warp Breaking Strength
Hexcel® HexForce™ 6543 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Tensile Impact 374 J/cm
700 ft-lb/in
Warp Breaking Strength
Hexcel® HexForce™ 7544 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Tensile Impact 374 J/cm
700 ft-lb/in
Filling Breaking Strength
Hexcel® HexForce™ 7544 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..