Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 374 J/cm | 700 ft-lb/in | Warp |
Hexcel® HexForce™ 328 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Tensile Impact | 374 J/cm | 700 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 3582 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 374 J/cm | 700 ft-lb/in | Warp |
Hexcel® HexForce™ 5328 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Tensile Impact | 374 J/cm | 700 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 6543 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 374 J/cm | 700 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 7544 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 374 J/cm | 700 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 7544 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |