Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 125 J/cm | 235 ft-lb/in | ASTM D1822 |
LyondellBasell Alathon® L5332CP High Density Polyethylene, Blow Molding Grade ALATHON L5332CP is bimodal molecular weight distribution, fractional melt index HDPE resin that exhibits an exceptional balance of environmental stress crack resistance and stiffness. Typical applic.. |