Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Critical Pressure = 13700 torr Product List

Chemical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Chemical Properties Metric English Comments
Critical Pressure 18.3 bar
13700 torr
Estimated
3M Fluorinert™ FC-72 Electronic Liquid
3M™ Fluorinert™ Liquid FC-72 is a non-conductive, thermally and chemically stable liquid ideal for many direct contact single and two phase low temperature heat transfer applications, in testing, ..