Chemical Properties | Metric | English | Comments |
---|---|---|---|
Carboxyl End Groups | 170 meq/kg | 170 meq/kg | Titration; Internal Method |
Solvay Specialty Polymers Veradel® 3600RP Polyethersulfone (PESU)
(Unverified Data**) Veradel® 3600RP hydroxyl-functionalized polyethersulfone (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersing .. |