Chemical Properties Metric English Comments
Acetaldehyde <= 0.100 ppm
<= 0.100 ppm
Limit; M2E-75-007
Indorama Ventures Mexico Polyclearâ„¢ Splash 3301 PET Resin
Description: La resina Polyclear® Splash PET 3301 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.74 dl/g. La resina Polyclear® Splash PET 3301 ha sido ..
Acetaldehyde 0.100 - 3.00 ppm
0.100 - 3.00 ppm
Average value: 1.23 ppm Grade Count:20
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..